Puas muaj qhov sib txawv ntawm huab cua tiv thaiv Q500NH hauv cov huab cua kub thiab huab cua huab cua thiab qhuav?

Huab cua tiv thaiv ntawm Q500NH hauv kub / vaum vs.

Q500nh ua txawv nyob rau hauv cov chaw ib puag ncig no vim yog ya raws thiab kub cuam tshuam ntawm MATINE tsim:

1. Kub & Huab Cua Huab Cua (piv txwv li, chaw sov, ntug hiav txwv)

Qhov Zoo:

Sai kev pib tshaj li pinina (3-6 lub hlis) vim nquag ntub / nthwv cua sov.

Kev sib tw:

Kev ua kom sov noo noo yuav ua rauzos pittingYog dej ntws tawm.

Ntau dua chloride / sulfate tso nyiaj (ntug dej / muaj) tuaj yeem cuam tshuam patina stability.

Corrosion tus nqi: 0.03-0.07 mm / xyoo tom qab muaj stabilization.

2. Cov huab cua qhuav (piv txwv li, Arid, Suab puam)

Qhov Zoo:

Tsawg tsawg corrosion (0.01-0.03 mm / xyoo) vim tias noo noo.

Sib npaug patina nrog tsaus dua, ntau ruaj khov.

Kev sib tw:

Sligle Patina tsim (12-24 lub hlis) vim yog ntub dej.

UV / thermal cycling yuav ua rau superficial oxide flaking (tsis muaj kev cuam tshuam ntawm kev cuam tshuam).


Cov Ntsiab Tseem Ceeb rau Kev Ua Haujlwm Zoo

Huab cua huab cua huab cua:

Tsim rautso kua mis(Zam kev ntxiab dej).

NtxivCorrosion Allowance(piv txwv li, {{+0.5 mm vs. qhuav zones).

Huab cua qhuav:

Nrawm Patination ntawmQee zaus dej txauthaum ntxov hauv kev pabcuam.

Cov Ntaub Ntawv Sib Piv:

Huab cua PATINE Tsim Sij Hawm Ruaj khov corrosion Yam txaus ntshai
Kub / vaum 3-12 lub hlis 0.03-0.07 mm / xyoo Pitting, Chlorides
Qhuav 1-2 xyoos 0.01-0.03 mm / xyoo Qeeb patina adhesion